Sink Marks in Injection Molding

Oct 22, 2026 Leave a message

JACKSON CHEN
JACKSON CHEN
Senior Product Development Engineer at Huizhou Jiejin Plastic Technology Co., Ltd., mold design, and custom manufacturing. Shares technical tutorials, process analyses, and professional tips and techniques for the plastics manufacturing industry.

Sink Marks in Injection Molding

 

Causes, Inspection and Prevention

Learn how part geometry, packing and cooling can contribute to sink marks in molded plastic components.

news-384-384

 

 

What Are Sink Marks in Injection Molding?

A sink mark is a localized depression on the surface of a molded plastic part. It often appears near a thicker section, such as a rib, boss or mounting feature.

 

As the plastic cools, it contracts. If a thick section shrinks differently from the surrounding material, the surface may pull inward and form a visible depression.

 

The correct solution depends on the part geometry, material, mold design and processing conditions.

 

1

Common Causes of Sink Marks

 

news-384-384

Thick Wall Sections

Thick regions cool more slowly and may shrink differently from thinner areas.

 
news-384-384

Packing and Cooling

Inadequate packing or uneven cooling may contribute to local shrinkage.

 

 

news-384-384

Ribs, Bosses and Geometry

Structural features may create thick local sections that require design review.

 

 

 

2

Sink Marks vs. Other Defects

Defect

Typical appearance

What to investigate

Sink mark

Localized shallow depression, often near a thick section or structural feature

Local wall thickness, packing, cooling and shrinkage

Void

Internal cavity within the part, which may not be visible from the outside

Thick-section cooling, material behavior and internal structure

Short shot

Part of the cavity is not completely filled

Filling behavior, material flow, venting and process conditions

Weld line

Visible line where separate melt-flow fronts meet

Gate location, flow pattern, melt condition and mold temperature

Flow mark

Visible streak or pattern associated with material flow

Filling behavior, temperature conditions and surface appearance

Flash

Excess material extends beyond the intended part boundary

Mold closure, parting line condition and process conditions

 

3

How to Inspect Sink Marks

 

 

       news-384-384news-574-231

 

4

How to Reduce Sink Marks

 

             Review wall thickness

news-36-29       Avoid unnecessary thick sections and abrupt transitions where the design permits.

 

              Optimize packing conditions

news-41-39     Check whether packing pressure and holding time are appropriate for the material and gate design.

 

              Review cooling

 news-30-35        Evaluate temperature distribution and cooling time before changing the production cycle.

 

               Inspect the mold design

news-40-33      Review gate location, cooling layout and the geometry around ribs and bosses.

 

      

5

 A Practical Troubleshooting Checklist

 

  1. Confirm the defect and acceptance criteria
  2. Review part geometry and wall thickness
  3. Verify the resin grade
  4. Record current molding conditions
  5. Evaluate gate and cooling design if needed
  6. Test changes under controlled conditions
  7. Inspect repeat samples and document results
  8.  

 

How JIEJIN PLASTIC Can Support Custom Plastic Parts

 

JIEJIN PLASTIC works with custom plastic parts, injection molding projects and 3D printing. For a new molded component, reviewing the part design, material requirements and appearance criteria early can help identify manufacturing considerations before production.

 

For an existing sink mark issue, drawings, defect photographs, material information and relevant dimensions can help establish what needs to be investigated. The root cause should be identified before recommending a specific correction.

 

image-20261016152239-35.jpeg

null

modular-1
Developing a Custom Plastic Part?

Discuss your part design, material requirements and manufacturing options with JIEJIN PLASTIC.

Frequently Asked Questions
 
 

What causes sink marks in injection molding?

 

-

Common contributors include thick sections, uneven cooling, insufficient packing and part geometry.

Can increasing packing pressure fix sink marks?

 

-

It may help in some cases, but excessive pressure can cause other defects. Adjustments should be validated against the full part specification.

Are sink marks the same as voids?

 

-

No. A sink mark is a surface depression, while a void is an internal cavity that may require additional inspection to identify.

Send Inquiry