Voids And Air Bubbles in Injection Molded Parts: Causes And Solutions

Nov 19, 2026 Leave a message

Voids and Air Bubbles in Injection Molded Parts: Causes and Solutions

 

Voids and air bubbles are common defects that can occur inside injection-molded plastic components.

Unlike surface defects such as flash, silver streaks or burn marks, internal voids may not be visible during a normal visual inspection.

They can appear as small empty spaces, bubbles or cavities inside the plastic material.

Depending on the product structure and application, internal voids may affect appearance, dimensional stability and mechanical performance.

news-1672-941

These defects are particularly important for transparent components, thick-walled plastic parts and products that require reliable structural strength.

 

Understanding the difference between gas bubbles and shrinkage-related voids is the first step toward identifying the correct solution.

 

This guide explains the main causes of internal bubbles and voids in injection molding and how manufacturers can prevent them.

 

 

 

1. What Are Voids and Air Bubbles in Injection Molding?

 

 

Voids and air bubbles are internal defects formed during the injection molding process.

 

Although the terms are sometimes used interchangeably, they do not always describe the same physical problem.

 

news-1536-1536
Voids

Voids are empty spaces or cavities inside a plastic component.

They are commonly associated with material shrinkage during cooling, especially in thicker sections where the outer material solidifies before the internal material has completed its shrinkage.

When insufficient packing material is available to compensate for this volume reduction, an internal cavity may develop.

 

news-1536-1536
Air Bubbles

Air bubbles are gas-filled spaces trapped inside the molded plastic.

They may result from trapped air, moisture vapor, volatile substances or other gas-related conditions during processing.

In some cases, the appearance of an internal bubble can resemble a shrinkage void.

The actual cause should be confirmed through part inspection and process investigation rather than visual appearance alone.

 

2. Common Causes of Internal Voids and Air Bubbles

 

2.1 Insufficient Packing Pressure

 

Packing pressure is used after the cavity has been filled to compensate for material shrinkage as the plastic cools.

 

If packing pressure is insufficient, additional material may not enter the cavity to compensate for shrinkage.

 

This can result in internal voids, particularly in thicker sections of the product.

 

Possible solutions:

  • Review packing pressure settings.
  • Evaluate the packing time.
  • Check whether the gate freezes too early.
  • Review product wall thickness.
  • Confirm that the mold is filled and packed consistently.

 

2.2 Thick Product Sections

 

Thick plastic sections cool more slowly than thin sections.

 

During cooling, the outside of a thick section may solidify first while the internal material continues to shrink.

 

If the shrinkage is not adequately compensated for, an internal void may form.

 

This is why product design plays an important role in preventing internal defects.

 

Possible solutions:

  • Avoid unnecessarily thick wall sections.
  • Use more uniform wall thickness where practical.
  • Consider coring out thick areas.
  • Use ribs to improve stiffness instead of increasing overall wall thickness.
  • Review packing conditions for thick features.

 

2.3 Moisture in Plastic Resin

 

Some plastic materials absorb moisture from the surrounding environment.

 

If moisture-sensitive resin is not dried according to the material supplier's recommendations, water vapor may contribute to gas-related defects during processing.

 

Materials such as PC, PA and certain PET-based grades require particular attention to drying conditions.

 

Possible solutions:

  • Verify the correct resin grade.
  • Check material storage conditions.
  • Follow the supplier's drying temperature and time recommendations.
  • Confirm dryer airflow and performance.
  • Avoid leaving dried material exposed to humid air for extended periods.

 

2.4 Trapped Air Inside the Mold Cavity

 

Air already present inside the cavity must escape as molten plastic enters.

 

If the venting system is insufficient, air may become trapped.

 

Depending on the location and filling conditions, this can contribute to gas-related defects or other surface problems.

 

Possible solutions:

  • Inspect mold venting channels.
  • Clean blocked vents.
  • Review the end-of-fill positions.
  • Evaluate product geometry and gate location.
  • Consider additional venting where required.

 

2.5 Unsuitable Injection Speed

 

Injection speed influences how the cavity fills and how air moves through the mold.

 

An unsuitable speed profile may contribute to air entrapment or unstable filling behavior.

 

However, injection speed should not be adjusted without considering mold venting, resin flow characteristics and product geometry.

 

Possible solutions:

  • Review the injection speed profile.
  • Run controlled filling trials.
  • Evaluate the location of gas-related defects.
  • Confirm that other processing conditions remain stable.

 

2.6 Excessive Material Temperature or Degradation

 

Excessive heat exposure may cause some plastics to degrade.

 

Degradation can generate gases or volatile substances that contribute to internal bubbles and other molding defects.

 

This risk may increase when the material remains in the heated barrel for too long or when processing temperatures exceed the suitable range for the resin.

 

Possible solutions:

  • Follow the resin supplier's processing recommendations.
  • Review barrel temperature settings.
  • Check residence time.
  • Avoid unnecessary heating during production interruptions.
  • Purge material when appropriate.

 

3. How to Identify the Difference Between Voids and Air Bubbles

 

Identifying the defect type is important because the corrective action may be different.

 

Inspection Observation

Possible Defect

Area to Investigate

Empty cavities inside thick sections

Shrinkage-related voids

Packing pressure, gate freeze and wall thickness

Small round gas pockets inside the material

Gas bubbles

Moisture, trapped gas and material condition

Bubbles in transparent plastic parts

Gas-related or shrinkage-related defect

Resin drying, filling and packing

Defects concentrated around thick bosses

Internal shrinkage voids

Product geometry and packing

Defects appear after material drying problems

Moisture-related bubbles

Dryer performance and resin storage

Defects occur at repeated mold locations

Mold venting or local flow issue

Cavity geometry and venting

 

For critical applications, further inspection methods may be required to confirm the internal structure of the part.

 

4. How to Prevent Voids and Air Bubbles

 

Prevention requires coordination between product design, mold engineering, material preparation and injection molding conditions.

 

Control Area

Recommended Action

Product design

Avoid unnecessarily thick sections

Wall thickness

Maintain more uniform wall thickness where practical

Packing pressure

Optimize packing conditions based on part geometry

Packing time

Confirm sufficient time before gate freeze

Material drying

Follow resin supplier recommendations

Mold venting

Ensure trapped air can escape

Injection speed

Optimize the filling profile

Material temperature

Avoid excessive heat exposure

Process monitoring

Record and review production conditions

 

No single parameter can solve every internal void or bubble problem.

 

A systematic approach is more reliable than randomly increasing pressure or temperature.

 

news-1672-941

 

5. How to Troubleshoot Internal Voids and Bubbles

 

When a molded component contains internal voids or bubbles, the following steps can help identify the cause.

 

1

Step 1: Locate the Defect

Determine whether the defect occurs in thick sections, near bosses, around ribs or across multiple areas.

2

Step 2: Review Product Wall Thickness

Check whether the defect is concentrated in areas with excessive material thickness.

Compare the actual part geometry with the 3D CAD model.

3

Step 3: Check Packing Conditions

 

Review packing pressure, packing time and the gate-freeze behavior.

Insufficient packing can contribute to shrinkage-related voids.

4

Step 4: Verify Resin Condition

 

Check whether the selected resin requires drying.

Review material storage, dryer settings and material handling procedures.

 

5

Step 5: Inspect Mold Venting

Check whether air can escape from the cavity effectively.

Inspect venting channels and potential air-trapping areas.

 

6

Step 6: Run Controlled Process Trials

 

Make adjustments one variable at a time.

Record the changes and compare the resulting parts to determine which adjustment improves the defect.

 

7

Step 7: Verify Product Performance

 

For parts with structural or functional requirements, visual improvement alone may not be sufficient.

Confirm that the product meets the relevant dimensional, mechanical and assembly requirements.

 

news-1424-800

 

 

6. Why Product Design Matters in Preventing Internal Voids

 

Internal voids are not always caused by machine settings.

 

In many cases, product geometry is an important contributing factor.

 

Thick sections, large bosses and sudden changes in wall thickness can create uneven cooling behavior.

 

When the outside of the product solidifies before the internal material has completed its shrinkage, voids may form.

 

During product design, engineers should consider:

  • Uniform wall thickness.
  • Proper rib dimensions.
  • Suitable boss design.
  • Smooth transitions between thick and thin areas.
  • Appropriate gate location.
  • Packing and cooling requirements.

 

Design for Manufacturability (DFM) review can help identify potential problems before the mold is manufactured.

 

7. Are Internal Voids Always a Reason to Reject a Plastic Part?

 

Not necessarily.

 

The acceptance of a part depends on its intended application and the severity of the defect.

 

 

For Example 

 

news-1536-1536

A small internal void in a non-structural decorative component may have limited impact.

news-1536-1536

A void near a screw boss may affect fastening strength.

news-1536-1536

A defect inside a transparent product may be unacceptable because it affects appearance.

news-1536-1536

A void in a load-bearing component may require additional performance evaluation.

 

Buyers and manufacturers should agree on product acceptance criteria before mass production.

 

For critical applications, functional testing and suitable inspection methods should be considered.

 

8. How JIEJIN PLASTIC Supports Custom Plastic Manufacturing

JIEJIN PLASTIC supports custom plastic product development, mold manufacturing, injection molding and 3D printing.

Our engineering team can review product drawings and discuss wall thickness, mold structure and manufacturing considerations before production.

For overseas OEM/ODM customers, we provide support throughout different stages of product development, including:

 

Our provide support

If you are developing a new plastic component or experiencing internal quality problems, you can share your product drawings and material requirements with our team for an initial review.

3D drawing review.

1

>>

Product structure evaluation.

2

>>

Mold design and manufacturing.

3

>>

Prototype development through 3D printing.

4

>>

Injection molding sample production.

5

>>

Mass production and delivery.

6

FAQ

 

 

image-20261016152239-27.jpeg

Q1: What causes air bubbles inside injection molded plastic parts?

Possible causes include moisture in the resin, trapped air, volatile substances and material degradation. The actual cause depends on the material and molding conditions.

Q2: What causes internal voids in thick plastic parts?

Internal voids are often related to shrinkage during cooling. If the internal material shrinks and packing pressure cannot compensate for the volume reduction, a cavity may develop.

Q3: Can increasing injection pressure eliminate internal voids?

Not always. Packing pressure and packing time may need adjustment, but increasing pressure without understanding the cause can create other defects or unnecessary stress.

Q4: Are air bubbles and silver streaks the same defect?

No. Silver streaks are visible surface marks, while internal bubbles are gas-filled spaces inside the material. They may share some causes, such as moisture or material degradation, but they are different defects.

Q5: Can product design help prevent internal voids?

Yes. More uniform wall thickness, properly designed ribs and bosses, and suitable gate placement can help reduce the risk of shrinkage-related voids.

Q6: How can internal bubbles be detected in opaque plastic parts?

Depending on the product requirements, manufacturers may use sectioning, microscopy, X-ray inspection or other suitable testing methods. The appropriate method depends on the component and inspection criteria.

 

 

Conclusion

 

 

news-2848-1600

 

Voids and air bubbles in injection molded parts can result from different mechanisms, including material shrinkage, moisture, trapped air and material degradation.

Identifying whether the defect is a shrinkage-related void or a gas-related bubble is essential before selecting a corrective action.

A reliable prevention strategy should combine suitable product design, material preparation, mold venting and stable packing conditions.

By reviewing these factors before mass production, manufacturers can reduce internal defects and improve the quality and consistency of custom plastic components.

news-2848-1600

image-20261016152234-13.jpeg

image-20261016152234-14.jpeg

null

modular-1
Looking for a Reliable Plastic Manufacturing Partner?

 Manufacturing Solutions by JIEJIN PLASTIC
Plastic Injection Molding · Plastic Parts · 3D Printing · Packaging Solutions

Send Inquiry

Send Inquiry